Excellent corrosion resistance in the water media of the extremely high temperature. Incoloy 926 Characteristic1.It has high resistance to pitting and crevice corrosion when in Halide and H2S contained acid media.2.In practice, effective in resistance of chloride stress corrosion cracking.3.A variety of corrosion have good corrosion resistance capability in the normal oxidation and restore environment.4.Upgrade mechanical properties than Cronifer 1925 LC-Alloy 904 L.5. Alloys has Improved the stability of metallurgical compared to a range of 18% of the nickel content alloys.6.With a certification of applied in manufacturing-related  pressure vessel VdTUV-196∼400 and ASME

Metallurgical structure926 is face-centered cubic lattice structure.

Corrosion resistance926 is an austenitic stainless steel alloy has a similar chemical composition with 904L alloy, its nitrogen content is 0.2%, molybdenum content is 6.5%. Molybdenum and nitrogen content significantly increased the resistance of pitting and crevice corrosion  in the halide media.Meantime, nickel and nitrogen not only ensures the stability of metallographical, but also reduce separating intergranular trend in the thermal process or welding process better than the nitrogen content of nickel alloy. 926 has particular corrosion resistance in the chloride ions medium due to the excellent local corrosion resistance and 25% nickel alloy content.A variety of experiments in the 10000-70000ppm of Chloride concentration, PH 5-6, 50-68 operating temperature of the slurry of limestone FGD system show that, after a 1-2 year trial period, 926 alloy without pitting and crevice corrosion.926 in other chemical media also has good corrosion resistance in the high temperature and high concentration of media, including sulfuric acid, phosphoric acid, acid gas, sea water, salt and organic acids.926 is the material that choosed for BAM directory Chapter 6 of "dangerous goods storage and transportation containers norms"  by  Berlin, Germany's national Institute for Materials Research and Testing (BAM) . In addition, in order to have the best corrosion resistance only when the material is in the right state of metallurgy and guarantee clean conditions.

Application fieldAlloy 926 is a multipurpose material can be applied in many industrial: 1. Fire system, water purification system, marine engineering and hydraulic piping perfusion system 2. The pipeline, joint, air systems in the acidic gas production 3. Evaporator, the heat exchanger, filter, mixer, etc. in the phosphate production4.Power plants condensation and pipe system in the use of sewage water to cool water5. The use of acidic organic catalyst chlorinated derivatives production 6. The production of cellulose pulp bleacher                                               7. Polished bar in the orrosive oil wells 8. Hose system in the ocean engineering                                                   9. Flue gas desulphurization system components 10. Sulfuric acid condensation and separation system                               11. Crystalline salt concentration and the evaporator 12. Transport of corrosive chemicals containers                                        13. Reverse osmosis desalination plant